Bitte benutzen Sie diese Kennung, um auf die Ressource zu verweisen: http://dx.doi.org/10.18419/opus-13218
Autor(en): Dreier, Julia
Brütting, Christian
Ruckdäschel, Holger
Altstädt, Volker
Bonten, Christian
Titel: Investigation of the thermal and hydrolytic degradation of polylactide during autoclave foaming
Erscheinungsdatum: 2021
Dokumentart: Zeitschriftenartikel
Seiten: 7
Erschienen in: Polymers 13 (2021), No. 2624
URI: http://nbn-resolving.de/urn:nbn:de:bsz:93-opus-ds-132374
http://elib.uni-stuttgart.de/handle/11682/13237
http://dx.doi.org/10.18419/opus-13218
ISSN: 2073-4360
Zusammenfassung: Polylactide (PLA) is one of the most important bioplastics worldwide and thus represents a good potential substitute for bead foams made of the fossil-based Polystyrene (PS). However, foaming of PLA comes with a few challenges. One disadvantage of commercially available PLA is its low melt strength and elongation properties, which play an important role in foaming. As a polyester, PLA is also very sensitive to thermal and hydrolytic degradation. Possibilities to overcome these disadvantages can be found in literature, but improving the properties for foaming of PLA as well as the degradation behavior during foaming have not been investigated yet. In this study, reactive extrusion on a twin-screw extruder is used to modify PLA in order to increase the melt strength and to protect it against thermal degradation and hydrolysis. PLA foams are produced in an already known process from the literature and the influence of the modifiers on the properties is estimated. The results show that it is possible to enhance the foaming properties of PLA and to protect it against hydrolysis at the same time.
Enthalten in den Sammlungen:04 Fakultät Energie-, Verfahrens- und Biotechnik

Dateien zu dieser Ressource:
Datei Beschreibung GrößeFormat 
polymers-13-02624.pdf1,14 MBAdobe PDFÖffnen/Anzeigen


Diese Ressource wurde unter folgender Copyright-Bestimmung veröffentlicht: Lizenz von Creative Commons Creative Commons