Bitte benutzen Sie diese Kennung, um auf die Ressource zu verweisen: http://dx.doi.org/10.18419/opus-13672
Langanzeige der Metadaten
DC ElementWertSprache
dc.contributor.authorAbitaev, Karina-
dc.contributor.authorAtanasova, Petia-
dc.contributor.authorBill, Joachim-
dc.contributor.authorPreisig, Natalie-
dc.contributor.authorKuzmenko, Ivan-
dc.contributor.authorIlavsky, Jan-
dc.contributor.authorLiu, Yun-
dc.contributor.authorSottmann, Thomas-
dc.date.accessioned2023-10-24T12:19:59Z-
dc.date.available2023-10-24T12:19:59Z-
dc.date.issued2023de
dc.identifier.issn2079-4991-
dc.identifier.other1869565533-
dc.identifier.urihttp://nbn-resolving.de/urn:nbn:de:bsz:93-opus-ds-136918de
dc.identifier.urihttp://elib.uni-stuttgart.de/handle/11682/13691-
dc.identifier.urihttp://dx.doi.org/10.18419/opus-13672-
dc.description.abstractZnO inverse opals combine the outstanding properties of the semiconductor ZnO with the high surface area of the open-porous framework, making them valuable photonic and catalysis support materials. One route to produce inverse opals is to mineralize the voids of close-packed polymer nanoparticle templates by chemical bath deposition (CBD) using a ZnO precursor solution, followed by template removal. To ensure synthesis control, the formation and growth of ZnO nanoparticles in a precursor solution containing the organic additive polyvinylpyrrolidone (PVP) was investigated by in situ ultra-small- and small-angle X-ray scattering (USAXS/SAXS). Before that, we studied the precursor solution by in-house SAXS at T = 25 °C, revealing the presence of a PVP network with semiflexible chain behavior. Heating the precursor solution to 58 °C or 63 °C initiates the formation of small ZnO nanoparticles that cluster together, as shown by complementary transmission electron microscopy images (TEM) taken after synthesis. The underlying kinetics of this process could be deciphered by quantitatively analyzing the USAXS/SAXS data considering the scattering contributions of particles, clusters, and the PVP network. A nearly quantitative description of both the nucleation and growth period could be achieved using the two-step Finke–Watzky model with slow, continuous nucleation followed by autocatalytic growth.en
dc.description.sponsorshipDeutsche Forschungsgemeinschaftde
dc.language.isoende
dc.relation.uridoi:10.3390/nano13152180de
dc.rightsinfo:eu-repo/semantics/openAccessde
dc.rights.urihttps://creativecommons.org/licenses/by/4.0/de
dc.subject.ddc540de
dc.titleIn situ ultra-small- and small-angle X-ray scattering study of ZnO nanoparticle formation and growth through chemical bath deposition in the presence of polyvinylpyrrolidoneen
dc.typearticlede
dc.date.updated2023-08-08T16:59:24Z-
ubs.fakultaetChemiede
ubs.fakultaetFakultätsübergreifend / Sonstige Einrichtungde
ubs.institutInstitut für Materialwissenschaftde
ubs.institutInstitut für Physikalische Chemiede
ubs.institutFakultätsübergreifend / Sonstige Einrichtungde
ubs.publikation.seiten19de
ubs.publikation.sourceNanomaterials 13 (2023), No. 2180de
ubs.publikation.typZeitschriftenartikelde
Enthalten in den Sammlungen:03 Fakultät Chemie

Dateien zu dieser Ressource:
Datei Beschreibung GrößeFormat 
nanomaterials-13-02180.pdfArtikel9,32 MBAdobe PDFÖffnen/Anzeigen
nanomaterials-13-02180-s001.zipSupplement769,65 kBUnknownÖffnen/Anzeigen


Diese Ressource wurde unter folgender Copyright-Bestimmung veröffentlicht: Lizenz von Creative Commons Creative Commons