Dynamics of poling PVDF between 25°C and 120°C
Files
Date
Authors
Journal Title
Journal ISSN
Volume Title
Publisher
Abstract
PVDF films with high β-content are poled in an electric field of 60 MV/m at temperatures between 25°C and 120°C. At 25°C the alignment of dipoles takes place in a central poling zone during several hours of poling. When the temperature is increased to 120°C the poling time necessary to align the dipoles in this narrow zone is reduced to several seconds. In addition, at temperatures higher than 90°C and increased poling times the central poling zone first increases but later decreases in its dielectric displacement. Simultaneously in a 10 μm regime adjoining the positive electrode a secondary displacement zone starts to grow. The strong reduction of this peak under short circuit conditions indicates hetero-charge accumulation in front of an anode.