Influence of a closed-loop controlled laser metal wire deposition process of S Al 5356 on the quality of manufactured parts before and after subsequent machining

dc.contributor.authorBecker, Dina
dc.contributor.authorBoley, Steffen
dc.contributor.authorEisseler, Rocco
dc.contributor.authorStehle, Thomas
dc.contributor.authorMöhring, Hans-Christian
dc.contributor.authorOnuseit, Volkher
dc.contributor.authorHoßfeld, Max
dc.contributor.authorGraf, Thomas
dc.date.accessioned2023-04-06T08:15:23Z
dc.date.available2023-04-06T08:15:23Z
dc.date.issued2021de
dc.date.updated2023-03-25T19:49:39Z
dc.description.abstractThis paper describes the interdependence of additive and subtractive manufacturing processes using the production of test components made from S Al 5356. To achieve the best possible part accuracy and a preferably small wall thickness already within the additive process, a closed loop process control was developed and applied. Subsequent machining processes were nonetheless required to give the components their final shape, but the amount of material in need of removal was minimised. The effort of minimising material removal strongly depended on the initial state of the component (wall thickness, wall thickness constancy, microstructure of the material and others) which was determined by the additive process. For this reason, knowledge of the correlations between generative parameters and component properties, as well as of the interdependency between the additive process and the subsequent machining process to tune the former to the latter was essential. To ascertain this behaviour, a suitable test part was designed to perform both additive processes using laser metal wire deposition with a closed loop control of the track height and subtractive processes using external and internal longitudinal turning with varied parameters. The so manufactured test parts were then used to qualify the material deposition and turning process by criteria like shape accuracy and surface quality.en
dc.description.sponsorshipMinistry of Science, Research and Arts of the Federal State of Baden-Württembergde
dc.description.sponsorshipProjekt DEALde
dc.identifier.issn0944-6524
dc.identifier.issn1863-7353
dc.identifier.other1843176653
dc.identifier.urihttp://nbn-resolving.de/urn:nbn:de:bsz:93-opus-ds-129349de
dc.identifier.urihttp://elib.uni-stuttgart.de/handle/11682/12934
dc.identifier.urihttp://dx.doi.org/10.18419/opus-12915
dc.language.isoende
dc.relation.uridoi:10.1007/s11740-021-01030-wde
dc.rightsinfo:eu-repo/semantics/openAccessde
dc.rights.urihttps://creativecommons.org/licenses/by/4.0/de
dc.subject.ddc670de
dc.titleInfluence of a closed-loop controlled laser metal wire deposition process of S Al 5356 on the quality of manufactured parts before and after subsequent machiningen
dc.typearticlede
ubs.fakultaetKonstruktions-, Produktions- und Fahrzeugtechnikde
ubs.institutInstitut für Strahlwerkzeugede
ubs.institutInstitut für Werkzeugmaschinende
ubs.publikation.seiten489-507de
ubs.publikation.sourceProduction engineering 15 (2021), S. 489-507de
ubs.publikation.typZeitschriftenartikelde

Files

Original bundle

Now showing 1 - 1 of 1
Thumbnail Image
Name:
s11740-021-01030-w.pdf
Size:
3.14 MB
Format:
Adobe Portable Document Format

License bundle

Now showing 1 - 1 of 1
No Thumbnail Available
Name:
license.txt
Size:
3.39 KB
Format:
Item-specific license agreed upon to submission
Description: