Autor(en): | Prass, Sebastian St-Pierre, J. Klingele, Matthias Friedrich, K. Andreas Zamel, Nada |
Titel: | Hydrogen oxidation artifact during platinum oxide reduction in cyclic voltammetry analysis of low-loaded PEMFC electrodes |
Erscheinungsdatum: | 2020 |
Dokumentart: | Zeitschriftenartikel |
Seiten: | 45-55 |
Erschienen in: | Electrocatalysis 12 (2021), S. 45-55 |
URI: | http://nbn-resolving.de/urn:nbn:de:bsz:93-opus-ds-133561 http://elib.uni-stuttgart.de/handle/11682/13356 http://dx.doi.org/10.18419/opus-13337 |
ISSN: | 1868-2529 1868-5994 |
Zusammenfassung: | An artifact appearing during the cathodic transient of cyclic voltammograms (CVs) of low-loaded platinum on carbon (Pt/C) electrodes in proton exchange membrane fuel cells (PEMFCs) was examined. The artifact appears as an oxidation peak overlapping the reduction peak associated to the reduction of platinum oxide (PtOx). By varying the nitrogen (N2) purge in the working electrode (WE), gas pressures in working and counter electrode, upper potential limits and scan rates of the CVs, the artifact magnitude and potential window could be manipulated. From the results, the artifact is assigned to crossover hydrogen (H2X) accumulating in the WE, once the electrode is passivated towards hydrogen oxidation reaction (HOR) due to PtOx coverage. During the cathodic CV transient, PtOx is reduced and HOR spontaneously occurs with the accumulated H2X, resulting in the overlap of the PtOx reduction with the oxidation peak. This feature is expected to occur predominantly in CV analysis of low-loaded electrodes made of catalyst material, whose oxide is inactive towards HOR. Further, it is only measurable while the N2 purge of the WE is switched off during the CV measurement. For higher loaded electrodes, the artifact is not observed as the electrocatalysts are not fully inactivated towards HOR due to incomplete oxide coverage, and/or the currents associated with the oxide reduction are much larger than the spontaneous HOR of accumulated H2X. However, owing to the forecasted reduction in noble metal loadings of catalyst in PEMFCs, this artifact is expected to be observed more often in the future. |
Enthalten in den Sammlungen: | 04 Fakultät Energie-, Verfahrens- und Biotechnik |
Dateien zu dieser Ressource:
Datei | Beschreibung | Größe | Format | |
---|---|---|---|---|
s12678-020-00627-6.pdf | 5,37 MB | Adobe PDF | Öffnen/Anzeigen |
Diese Ressource wurde unter folgender Copyright-Bestimmung veröffentlicht: Lizenz von Creative Commons