Bitte benutzen Sie diese Kennung, um auf die Ressource zu verweisen: http://dx.doi.org/10.18419/opus-14530
Langanzeige der Metadaten
DC ElementWertSprache
dc.contributor.authorKlostermann, Sina V.-
dc.contributor.authorKappler, Julian-
dc.contributor.authorWaigum, Alexander-
dc.contributor.authorBuchmeiser, Michael R.-
dc.contributor.authorKöhn, Andreas-
dc.contributor.authorKästner, Johannes-
dc.date.accessioned2024-06-17T12:02:13Z-
dc.date.available2024-06-17T12:02:13Z-
dc.date.issued2024de
dc.identifier.issn1463-9076-
dc.identifier.issn1463-9084-
dc.identifier.other1892312859-
dc.identifier.urihttp://nbn-resolving.de/urn:nbn:de:bsz:93-opus-ds-145492de
dc.identifier.urihttp://elib.uni-stuttgart.de/handle/11682/14549-
dc.identifier.urihttp://dx.doi.org/10.18419/opus-14530-
dc.description.abstractLithium–sulfur batteries (LSBs) have attracted attention due to their high theoretical energy density. This and various other advantages, such as the availability and non-toxicity of sulfur, raise interest in LSBs against the background of the energy revolution. However, a polysulfide shuttle mechanism can adversely affect the electrochemical performance of the cell. The sulfur redox properties are influenced, for example, by the electrolyte and the cathode material. Here, a computational study of the discharge process of an LSB with sulfurized poly(acrylonitrile) (SPAN) as the cathode material in combination with a carbonate electrolyte is presented. The nucleation of produced solid Li2S is compared to soluble Li2S. Dominating species are determined by comparing the Gibbs free energy of several species. We found that multiple lithiation steps occur before each Li2S detachment, preventing longer-chain polysulfide cleavage and a polysulfide shuttle. Through nucleating on the nitrogen-rich backbone of SPAN, Li2S units are stabilized by interactions with each other and with the nitrogen atoms. Experimental data show a potential drop and plateau during discharge, which is consistent with the calculated discharge profiles of SPAN with both soluble and nucleated Li2S, and hints at a direct solid-solid transition in the Li-SPAN cell during discharge when using carbonate-based electrolytes.en
dc.description.sponsorshipDeutsche Forschungsgemeinschaftde
dc.description.sponsorshipStuttgart Center for Simulation Sciencede
dc.description.sponsorshipState of Baden-Württembergde
dc.language.isoende
dc.relation.uridoi:10.1039/d3cp06248ade
dc.rightsinfo:eu-repo/semantics/openAccessde
dc.rights.urihttps://creativecommons.org/licenses/by/3.0/de
dc.subject.ddc540de
dc.titleThe reduction behavior of sulfurized polyacrylonitrile (SPAN) in lithium-sulfur batteries using a carbonate electrolyte : a computational studyen
dc.typearticlede
dc.date.updated2024-04-25T13:22:28Z-
ubs.fakultaetChemiede
ubs.institutInstitut für Polymerchemiede
ubs.institutInstitut für Theoretische Chemiede
ubs.publikation.seiten9998-10007de
ubs.publikation.sourcePhysical chemistry, chemical physics 26 (2024), S. 9998-10007de
ubs.publikation.typZeitschriftenartikelde
Enthalten in den Sammlungen:03 Fakultät Chemie

Dateien zu dieser Ressource:
Datei Beschreibung GrößeFormat 
D3CP06248A.pdf1,55 MBAdobe PDFÖffnen/Anzeigen


Diese Ressource wurde unter folgender Copyright-Bestimmung veröffentlicht: Lizenz von Creative Commons Creative Commons